Why a screen proof is not enough
A colour on a monitor is emitted light; a colour on fabric is reflected light through a dyed or coated surface. The same hex value looks different on a phone, a paper proof and a stretch polyester jersey, and none of those shows how the kit behaves in daylight or under floodlights.
For a club kit, the colour has to work as a set: jersey, bib shorts, cap, socks and trim. Each material takes colour differently, so each is approved as part of the same reference, not as an isolated artwork file.
That is why the approval step is a physical swatch or a decorated panel, not a PDF.
Base shade and sublimation
Dye sublimation prints into the fabric, so the base shade is part of the final colour. A bright white base reads cooler and more saturated; a tinted base warms the same artwork. On dark bases, the artwork needs more density to hold its value.
This matters most on light colours — pale grey, sky blue, mint and white panels — where a small shift in the base is visible across a large jersey back. It matters on gradients too, where the transition has to stay smooth on the actual knit.
The approved sample should be made from the production fabric, not from a substitute that happens to be in the sample room.
How a colour is approved
The method depends on the finish. Solid fabrics are matched with a lab dip; sublimated panels are checked with a strike-off printed on the production base. Both are compared against your reference under controlled light.
Two checks are worth doing:
- Daylight and indoor light: a colour that matches at the window can shift under warm indoor lighting.
- Side by side: compare the swatch with the reference on the same surface, not from memory or from two screens.
Once approved, the swatch is labelled and kept with the order file. That is the reference the bulk fabric check is measured against.
Matching the whole kit
A jersey and its bib shorts are usually different fabrics: a light stretch knit against a compressive knit. The same colour will not print identically on both unless it is matched as a set.
Ask for the panels to be checked together — jersey front and back, bib short leg, cap and socks — rather than one at a time. A black that reads neutral on the jersey can read blue on the bib short if the base fabrics differ.
Trim adds another variable. Zip tape, gripper silicone, binding tape and thread all need a reference, especially on a two-colour kit where the accent is repeated across five pieces.
What changes between lots
Yarn lots, dye baths and heat-press conditions all move colour slightly. The purpose of a tolerance is to define how much movement is acceptable before a lot is rejected, rather than expecting an exact numerical match on every roll.
During production, fabric is checked for shade, weight and hand-feel against the approved swatch before cutting. If a lot sits outside the tolerance, it is raised before it becomes a finished garment.
The same record protects a repeat order. The second run is compared with the approved swatch, not with a photograph of the first delivery. Send references through the contact page, or start from the colourways in the catalog.